Phenomenological tracking of pitting corrosion and the mechanical integrity of a magnesium rare earth alloy

Research output: Chapter in Book or Conference Publication/ProceedingConference Publicationpeer-review

Original languageEnglish (Ireland)
Title of host publicationBioabsorbable Metals 2021
Place of PublicationAlicante, Spain (online)
Publication statusPublished - 1 Aug 2021

Authors (Note for portal: view the doc link for the full list of authors)

  • Authors
  • van Gaalen, Kerstin and Gremse, Felix and Benn, Florian and Kopp, Alexander and Vaughan, Ted

Cite this