Skip to main navigation Skip to search Skip to main content

Fibrous composite matrix characterisation using nanoindentation: The effect of fibre constraint and the evolution from bulk to in-situ matrix properties

Research output: Contribution to a Journal (Peer & Non Peer) › Article › peer-review

Original languageEnglish (Ireland)
Number of pages7
JournalComposites Part A: Applied Science and Manufacturing
Volume68
Publication statusPublished - 1 Jan 2015